Heißes Produkt

ASTM Nickellegierung 718/UNS N07718 WILTED RHE mit geglühter und eingelegter Oberfläche

Kurzbeschreibung:

Alloy 718 is an age-hardenable nickel-chromium alloy that combines corrosion resistance with high strength and good fabricability. It has high creep-rupture strength at temperatures up to 700℃. Its excellent relaxation resistance contributes to its application in springs.



Produktdetail

Produkt -Tags

Grad: Alloy 718 /N07718, Alloy 625 /N06625 , Alloy 600 /N06600 ,Alloy 601 /N06601 ,  Alloy C276 /N10276 , Alloy 800 /N08800 , Alloy 825 /N08825 , Alloy 400 /N04400,etc

Standard: ASTM B517 ,ASTM B775, ASTM B516, ASTM B751, ASTM B619, ASTM B725, ASTM B730, etc

Oberfläche: Annealed Pickled/ Bright Annealed

Technologie: PAW/GTAW

Ndt: Radiographic test; Penetrant test; Hydrostatic test; Eddy current test; Ultrasonic test

Inspektion: 100% RT

Verpackung: Plywooden Case

Qualitätssicherung: ISO & Ped

IMG_20220224_151023

Alloy 718 / UNS N07718 Chemical Composition:

%

Ni

Fe

Cr

Mo

C

Mn

Si

P

S

Co

NB+Ta

Ti

Al

Cu

B

min

50.0

Gleichgewicht

17.0

2.80

-

-

-

-

-

-

4.75

0.65

0.20

-

-

Max

55.0

21.0

3.30

0.08

0.35

0.35

0.015

0.015

1.00

5.50

1.15

0.80

0.30

0.006

Physische Eigenschaften:

Dichte8,23 g/cm3
Schmelzbereich1260-1335℃

 

Merkmale: Alloy 718 is an age-hardenable nickel-chromium alloy that combines corrosion resistance with high strength and good fabricability. It has high creep-rupture strength at temperatures up to 700℃. Its excellent relaxation resistance contributes to its application in springs.

Anwendungen: Gasturbinenmotoren, Raketenmotoren, Kernreaktoren und Raumfahrzeuge.